Jointing Sand Washout Stopped on a Tobermore Fusion Patio with a GftK VDW 855 Resin

January 27, 2025 by Consumer Team · 7 min read

After two winters of sand streaming out of 5mm joints on a Tobermore Fusion patio, the repair moved to GftK VDW 855, a two-component epoxy resin grout rated from 3mm joint widths upward. The terrace carried a 1:60 fall toward an ACO-style channel, with each heavy rain pushing pale silica fines into the planting bed.

Jointing Sand Washout Stopped on a Tobermore Fusion Patio with a GftK VDW 855 Resin

The Tobermore Fusion flags on this job were laid in 2021 across a 42 square metre terrace with a nominal 1:60 fall running toward the lower boundary. The original jointing was kiln-dried silica sand brushed into 5mm joints. By the second autumn, the sand had migrated. Rainwater sheeting down the fall was lifting fines from the upper joints and leaving a fan of silt across the two lowest courses and the adjacent bed.

The replacement specified was GftK VDW 855, a two-part epoxy resin jointing compound. Within the GftK range it is among the few products rated for use on falls and around drainage channels without slumping, which mattered because the pitch is continuous and the whole terrace drains to a single ACO-style linear channel at the low edge.

Why kiln-dried sand moved

Kiln-dried sand stays in place through friction and a slight moisture-bound crust, which can last through much of the year on a level patio yet breaks down quickly once water is driven along a 1:60 fall. Sheet flow across the surface finds the joint lines, and the Fusion flag has a fairly smooth wearing course. By the third or fourth course, the water was moving fast enough to entrain the top few millimetres of sand and carry it downhill.

The evidence was visible before any flag was lifted. Every joint on the upper half of the terrace had recessed by 4mm to 8mm below the arris. The lowest three courses showed sand heaped proud of the joints, and the border soil had a pale silica cap.

A permeable sub-base alone would not have corrected this failure, because the movement was happening across the surface. Infiltration was not the mechanism driving the loss of sand. The bedding here was a semi-dry mortar screed over a Type 1 sub-base, so the joints were not providing meaningful vertical drainage.

Once the upper joints emptied, water began tracking along the bedding interface. Two flags near the head of the fall had started to rock under load, and each freeze cycle would have accelerated that movement.

Cutting out the sand and preparing the joints

The old sand had to be removed completely. VDW 855 needs a dry joint, because damp fines interfere with the epoxy cure. Any sand left behind also reduces the resin depth and creates a weak plane inside the joint.

The joints were raked out with a 4mm oscillating multi-tool blade, then vacuumed twice with a wet-and-dry vacuum drawn along each line. The aim was to leave clean arrises and a full-depth void, without loose fines sitting on the bedding shoulder.

GftK specifies a minimum joint depth of 30mm for trafficked areas and no less than the flag thickness minus the bedding contact on pedestrian patios. The Fusion flags here are 50mm thick, which left ample depth after the sand was cleared.

The two rocking flags were lifted. Their bedding was cut back and re-laid on a fresh slurry-primed screed. Raimondi levelling wedges held them flush to the neighbouring arris while the mortar went off, then snapped cleanly at the base after cure so nothing remained in the joint to foul the resin.

Where the original bedding was still sound, a Marshalls-type slurry primer was worked into the flag edges and the exposed bedding shoulder. On porcelain patio installation, priming is the usual failure point. Fusion is a wet-cast concrete flag, so the resin keys to it more readily than it would to a glazed porcelain edge. The slurry also created a consistent bond line and stopped epoxy leaching into the porous bedding before it gelled.

The product choice also matched the geometry of the terrace. VDW 855 is workable down to 3mm joint widths and is pot-stable on falls up to roughly 1:40. That gave enough tolerance for the 5mm Fusion joints and the existing 1:60 fall, while avoiding the downhill washout that had emptied the sand.

A fully flexible jointing compound was the comparison left on the table for this screed bed. GftK rates the 855 well beyond a decade in trafficked commercial work, although those figures come from rigid bases. This terrace sits on a mortar screed that can still move a fraction with ground conditions, so the resin bond at the arris carries more responsibility than it would on a fully rigid build.

Mixing and placing the VDW 855

The 855 comes as a resin and hardener that are combined immediately before use, then blended with the graded aggregate supplied in the pack. Working time drops sharply on a warm day, so the 42 square metres were divided into three pours of roughly 14 square metres each. The aggregate was pre-weighed for every batch before mixing began.

Once mixed, the compound was tipped onto the flags in a ribbon and pulled across the joints with a hard rubber squeegee held at a low angle. The direction of travel mattered on the fall. Working across the slope kept the material sitting in the joints instead of letting it run toward the low end.

Each joint was struck twice. The second pass crossed the first at ninety degrees, which helped drive out trapped air that would otherwise show as pinholes after cure.

As the surface film began to matte, a soft coco broom was swept diagonally over the flags to lift the excess resin skin from the face. Brooming before the film had tightened would have pulled material back out of the joints. Leaving the film too long would have allowed haze to cure onto the wearing course. On this Fusion surface the workable clean-up window was about twenty minutes at 18 degrees, and it tightened fast above 22 degrees.

A second, lighter brooming an hour later cleared the last of the sheen. At the low edge, the resin was tooled back cleanly from the ACO grating. No epoxy was allowed to bridge the flag and the channel lip, because that bridge would have carried movement across the expansion gap and cracked the joint within a season.

Reading the fall against the channel

A 1:60 fall is at the low end for reliable water shedding on a smooth concrete flag. For a garden path fall or a terrace of this size, 1:40 to 1:50 gives more margin. The existing structure was fixed, and re-grading was not on the table.

The compensation was to confirm that the linear channel at the foot of the slope could take the whole surface flow. Once the resin joints were sealed, water no longer dispersed downward in the limited way it had through the failed sand.

Resin jointing on a non-permeable bed converts the joints from a minor secondary drainage route into a sealed surface. Every litre that lands on the terrace now reports to the channel. Before the pour, the channel outfall was checked for fall and connection, because a sealed patio draining to an undersized or silted channel simply shifts standing water from the joints onto the paving surface.

A genuinely permeable paver sub-base would need a different specification: open-graded jointing aggregate, a permeable laying course, and a sub-base built to store and release water. That was never the construction under this terrace. The decision to use resin depended on recognising the mortar screed and the fixed channel as the working drainage system.

What the first winter showed

Through the following wet season, the joints held with no recession and no silt fan in the border. The two re-bedded flags stayed flush, and the channel cleared the surface flow without ponding along the low courses. The repair still leaves the resin bond at the arris doing the work each time the screed takes up minor ground movement.

Previous article 7 Bee-Attracting Plants the RHS Recommends for Chalk Soil Read article